Simple fabrication of highly ordered AAO nanotubes

dc.contributor.authorTasaltin, N.
dc.contributor.authorOzturk, S.
dc.contributor.authorYuzer, H.
dc.contributor.authorOzturk, Z. Z.
dc.date.accessioned2025-10-29T11:36:58Z
dc.date.issued2009
dc.departmentFakülteler, Temel Bilimler Fakültesi, Fizik Bölümü
dc.description.abstractIn this paper, simple fabrication of hexagonally well-ordered Anodic Aluminium Oxide (AAO) nanotubes with high aspect ratio was reported. AAO nanotubes were obtained by two-step anodization. High purity aluminium foils were anodized in oxalic acid solution by applying 40 V constant voltage at 0 degrees C for 30 min. Removing of AAO barrier layer was discussed in details. AAO nanotubes were characterized by Scanning Electron Microscopy (SEM). SEM micrographs show that fabricated AAO nanotubes are approximately 70 nm in diameters and 9 mu m in lengths with 90 nm interpore distances in a relatively large area of about 2 cm(2). Fabricated AAO nanotubes have high aspect ratio approximately 130.
dc.description.sponsorshipThe Scientific and Technological Research Council of Turkey [106T546]
dc.description.sponsorshipThis study was supported by Grant No. 106T546 from The Scientific and Technological Research Council of Turkey.
dc.identifier.endpage84
dc.identifier.issn2066-0049
dc.identifier.issue1
dc.identifier.startpage79
dc.identifier.urihttps://hdl.handle.net/20.500.14854/13571
dc.identifier.volume1
dc.identifier.wosWOS:000219370500011
dc.identifier.wosqualityN/A
dc.indekslendigikaynakWeb of Science
dc.language.isoen
dc.publisherVirtual Inst Physics
dc.relation.ispartofJournal of Optoelectronic and Biomedical Materials
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WOS_20251020
dc.subjectAnodization
dc.subjectAnodic aluminium oxide
dc.subjectAAO template
dc.subjectNanotubes
dc.titleSimple fabrication of highly ordered AAO nanotubes
dc.typeArticle

Dosyalar