Sintering behavior of ZnO:Al ceramics fabricated by sol-gel derived nanocrystalline powders
Yükleniyor...
Tarih
Dergi Başlığı
Dergi ISSN
Cilt Başlığı
Yayıncı
Wiley-V C H Verlag Gmbh
Erişim Hakkı
info:eu-repo/semantics/closedAccess
Özet
ZnO:Al ceramics (Zn:Al, 0.95:0.05) were prepared by using sol-gel derived nanocrystalline powders. XRD patterns of the doped ceramics revealed the existence of both zincite (JCPDS 36-1451) and gahnite (JCPDS 5-0669) phases. Gahnite phase (ZnAl2O4) was segregated along the ZnO grain boundaries. At the sintering temperature of 1200 degrees C, relative density of the undoped and Al doped ceramics were measured as 0.695 and 0.628, respectively. Both grain size and relative density of the ceramics decreased with Al doping. (C) 2009 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim
Açıklama
Anahtar Kelimeler
ZnO, sol-gel, microstructure-final, ceramic
Kaynak
Crystal Research and Technology
WoS Q Değeri
Scopus Q Değeri
Cilt
44
Sayı
9