Fretting wear of ZrN and Zr(21% Hf)N coatings

dc.contributor.authorAtar, E
dc.contributor.authorÇimenoglu, H
dc.contributor.authorKayali, ES
dc.date.accessioned2025-10-29T11:08:08Z
dc.date.issued2004
dc.departmentFakülteler, Temel Bilimler Fakültesi, Matematik Bölümü
dc.description8th Conference of the European-Ceramic-Society -- JUN 29-JUL 03, 2003 -- Istanbul, TURKEY
dc.description.abstractIn this study, the wear behaviours of ZrN and Zr(21% Hf)N coatings, deposited on hardened AISI D2 cold work tool steel were examined by a fretting wear tester. The hardness of ZrN and Zr(21% Hf)N coatings were almost the same, where as they exhibited different wear resistance. Addition of 21% Hf to ZrN coating achieved about 25 IN, increase in the wear resistance.
dc.description.sponsorshipTurkish Ceram Soc,European Ceram Soc
dc.identifier.doi10.4028/www.scientific.net/KEM.264-268.477
dc.identifier.endpage480
dc.identifier.isbn0-87849-946-6
dc.identifier.issn1013-9826
dc.identifier.orcid0000-0002-8157-5556
dc.identifier.orcid0000-0002-9921-7108
dc.identifier.scopus2-s2.0-8744250316
dc.identifier.scopusqualityQ4
dc.identifier.startpage477
dc.identifier.urihttps://doi.org/10.4028/www.scientific.net/KEM.264-268.477
dc.identifier.urihttps://hdl.handle.net/20.500.14854/5237
dc.identifier.volume264-268
dc.identifier.wosWOS:000223059700113
dc.identifier.wosqualityN/A
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherTrans Tech Publications Ltd
dc.relation.ispartofEuro Ceramics Viii, Pts 1-3
dc.relation.publicationcategoryKonferans Öğesi - Uluslararası - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WOS_20251020
dc.subjectZrN coating
dc.subjectHafnium
dc.subjectwear
dc.subjectPVD coating
dc.subjectfretting
dc.titleFretting wear of ZrN and Zr(21% Hf)N coatings
dc.typeConference Object