Two significant factors affecting the dimensions of the zno nanorods during chemical bath deposition: Precursor solution concentration and hmta content

dc.contributor.authorKardeş, Memnune
dc.contributor.authorÖztürk, Koray
dc.date.accessioned2025-10-29T12:08:51Z
dc.date.issued2023
dc.departmentGebze Teknik Üniversitesi
dc.description.abstractThe effects of zinc ion concentration and hexamethylene tetramine (HMTA) content of the aqueous precursor solution on the aspect ratios of the one-dimensional (1D) ZnO nanorods during chemical bath deposition (CBD) were investigated. The ZnO nanorods were grown on these seeded substrates by the low-temperature CBD method at 95 °C for 5 h. In the first part of this investigation the zinc nitrate hexahydrate (ZNH) to HMTA molar ratio was kept constant at a ratio of 1:1 for each of the CBD solutions prepared with different Zn+2 ion concentrations of 0.025, 0.035, 0.050, and 0.075 M. The number densities of the nanorods (i.e., number of nanorods per unit area) were increased with the increasing concentration. In the second part, the ZNH to HMTA molar ratio was varied to differ from the 1:1 value and, in turn, to obtain the precursor solutions relatively rich in Zn+2 or OH?ions. Here, the concentration of the precursor solution was kept constant at 0.05 M. The lateral growth perpendicular to the c-axis of the ZnO nanorods was found to be suppressed with the increasing HMTA content (e.g., for the ZNH to HMTA molar ratio of 0.4: 1) due to its capping effect. However, the precursor solution containing an excessive amount of HMTA led to a decrease in the probability of crystal growth, which has been attributed to the OH? ion enrichment. © 2025 Elsevier B.V., All rights reserved.
dc.identifier.doi10.16984/saufenbilder.1241020
dc.identifier.endpage767
dc.identifier.issn2147-835X
dc.identifier.issn1301-4048
dc.identifier.issue4
dc.identifier.scopus2-s2.0-85218783309
dc.identifier.scopusqualityN/A
dc.identifier.startpage757
dc.identifier.trdizinid1194027
dc.identifier.urihttps://doi.org/10.16984/saufenbilder.1241020
dc.identifier.urihttps://search.trdizin.gov.tr/tr/yayin/detay/1194027
dc.identifier.urihttps://hdl.handle.net/20.500.14854/14724
dc.identifier.volume27
dc.indekslendigikaynakScopus
dc.indekslendigikaynakTR-Dizin
dc.language.isoen
dc.publisherSakarya University
dc.relation.ispartofSakarya University Journal of Science
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.snmzKA_Scopus_20251020
dc.subjectAspect ratio
dc.subjectCBD
dc.subjectCrystal growth
dc.subjectHMTA
dc.subjectZnO nanorods
dc.titleTwo significant factors affecting the dimensions of the zno nanorods during chemical bath deposition: Precursor solution concentration and hmta content