Atomic layer deposited zinc oxide thin film on pencil graphite for DNA sensor applications

dc.contributor.authorGungor, Mustafa Ali
dc.contributor.authorAlev, Onur
dc.contributor.authorKaya, Hilmi Kaan
dc.contributor.authorArslan, Leyla Colakerol
dc.contributor.authorBuyukkose, Serkan
dc.contributor.authorOzturk, Zafer Ziya
dc.contributor.authorKuralay, Filiz
dc.date.accessioned2025-10-29T11:24:06Z
dc.date.issued2023
dc.departmentFakülteler, Temel Bilimler Fakültesi, Kimya Bölümü
dc.departmentFakülteler, Temel Bilimler Fakültesi, Fizik Bölümü
dc.description.abstractAtomic Layer Deposition (ALD) enables precise thin-film deposition on electrode substrates for electrochemical sensors. In this work, we present the first example of ALD grown zinc oxide (ZnO) deposition on pencil graphite surfaces for deoxyribonucleic acid (DNA) sensory applications, including its detection and DNA damage investigation. For DNA sensing studies, the use of highly productive materials is essential. In this context, the ZnO modified pencil graphite electrodes (ZnO/PGEs) exhibited good electrochemical properties that make them a suitable substrate. ZnO films were characterized using scanning electron microscopy (SEM), ultraviolet-visible (UV-Vis) spectroscopy, photoluminescence (PL), X-ray photoelectron spectroscopy (XPS), and electrochemical methods. The DNA recognition capability of the thin film coated electrodes was tested by using differential pulse voltammetry (DPV), which showed a linear response ranging from 1 mg L-1 to 200 mg L-1 based on the oxidation of guanine (G) with a limit of detection value (LOD) of 0.53 mg L-1 (n = 3). In addition to this, impedimetric monitoring of oxidative DNA damage was performed in the presence of copper(II)/hydrogen peroxide (Cu(II)/H2O2) reagents, and protection studies were conducted in the presence of ascorbic acid. ZnO thin film-based electrodes exhibited good sensor performance in terms of sensitivity, stability, and reproducibility.
dc.identifier.doi10.1016/j.mtcomm.2023.106776
dc.identifier.issn2352-4928
dc.identifier.orcid0000-0002-5301-679X
dc.identifier.orcid0000-0003-0356-9692
dc.identifier.orcid0009-0002-4562-7379
dc.identifier.scopus2-s2.0-85169831491
dc.identifier.scopusqualityQ2
dc.identifier.urihttps://doi.org/10.1016/j.mtcomm.2023.106776
dc.identifier.urihttps://hdl.handle.net/20.500.14854/9756
dc.identifier.volume36
dc.identifier.wosWOS:001060922600001
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherElsevier
dc.relation.ispartofMaterials Today Communications
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WOS_20251020
dc.subjectAtomic layer deposition
dc.subjectDNA
dc.subjectOxidative DNA damage
dc.titleAtomic layer deposited zinc oxide thin film on pencil graphite for DNA sensor applications
dc.typeArticle